Abstract

In this paper were conducted virtual tests to assess the impact of geometry changes on the response of metallic hexagonal honeycomb structures to applied loadings. The lateral compressive stress state was taken into consideration. The material properties used to build numerical models were assessed in laboratory tests of aluminium alloy 7075. The modelling at meso-scale level allow to comprehensive study of honeycomb internal structure. The changes of honeycomb geometry elements such as: fillets radius of the cell edges in the vicinity of hexagonal vertexes, wall thickness were considered. The computations were conducted by using finite element method with application of the ABAQUS finite element method environment. Elaborated numerical models allowed to demonstrate sensitivity of honeycomb structures damage process response to geometry element changes. They are a proper tools to perform optimization of the honeycomb structures. They will be also helpful in designing process of modern constructions build up of the considered composite constituents in various branches of industry. Moreover, the obtained results can be used as a guide for engineers. Conducted virtual tests lead to conclusion that simplification of the models of internal honeycomb structure which have become commonplace among both engineers and scientist can lead to inaccurate results.
Go to article

Abstract

Heating of steel or structural aluminum alloys at a speed of 2 to 50 K/min – characterizing the fire conditions – leads to a reduction in mechanical properties of the analyzed alloys. The limit of proportionality fp, real fy and proof f₀₂ yield limit, breaking strength fu and longitudinal limit of elasticity E decrease as the temperature increases. Quantitative evaluation of the thermal conversion in strengths of structural alloys is published in Eurocodes 3 and 9, in the form of dimensionless graphs depicting reduction coefficients and selected (tabulated) discrete values of mechanical properties. The author’s proposal for an analytical formulation of code curves describing thermal reduction of elasticity modulus and strengths of structural alloys recommended for an application in building structures is presented in this paper.
Go to article

Abstract

Ceramic injection moulding and gas pressure infiltration were employed for the manufacturing of alumina/AlSi10Mg composites. Porous ceramic preforms were prepared by mixing alumina powder with a multi-binder system and injection moulding of the powder polymer slurry. Then, the organic part was removed through a combination of solvent and thermal debinding, and the materials were finally sintered at different temperatures. The ceramic preforms manufactured in this way were infiltrated by an AlSi10Mg alloy. The microstructure and properties of the manufactured materials were examined using scanning electron microscopy, mercury porosimetry and bending strength testing. The results of transmission electron microscopy and scanning electron microscopy observations show that the fabricated composite materials are characterised by the percolation type of the microstructure and a lack of unfilled pores with good cohesion at the metal-ceramic interfaces. This is surprising considering that over 30% of the pores are smaller than 1 μm. The results show that the bending strength of the obtained composites decreased with increasing sintering temperature of the porous preforms.
Go to article

Abstract

The herein paper contains the results of investigations on a new type of cellulose blend used for the manufacture of profiles applied in the process of making gating systems in the foundry industry. A standard cellulose profile was subjected to an experiment. During the experiment the profile was filled with a liquid cast iron and at the same time the temperatures of the liquid metal crystallizing inside the profile were measured as well as the temperature of the outer layer of the profile was controlled. Further, the microstructure of the cast iron, which crystallized out inside the cellulose profile, was analysed and the cellulose, thermally degraded after the experiment, was verified with the use of the chemical analysis method. Moreover, a quality analysis of the original as well as the degraded cellulose profile was run with the use of the FTIR infrared spectroscopy. The presented results revealed that the cellulose blend is aluminium silicate enriched and contains organic binder additives. The cast iron, which crystallized out, tended to have an equilibrium pearlitic structure with the release of graphite and carbides. The generation of disequilibrium ausferrite phases was also observed in the structure.
Go to article

Abstract

A comprehensive understanding of melt quality is of paramount importance for the control and prediction of actual casting characteristics. Among many phenomenon that occur during the solidification of castings, there are four that control structure and consequently mechanical properties: chemical composition, liquid metal treatment, cooling rate and temperature gradient. The cooling rate and alloy composition are most important among them. This paper investigates the effect of the major alloying elements (silicon and copper) of AlSi-Cu alloys on the size of secondary dendrite arm spacing. It has been shown that both alloying elements have reasonable influence on the refinement of this solidification parameter
Go to article

Abstract

With the increase in wall thickness of the casting of iron-nickel-aluminium-bronze, by the reduction of the cooling rate the size of κII phase precipitates increases. This process, in the case of complex aluminium bronzes with additions of Cr, Mo and W is increased. Crystallization of big κII phase, during slow cooling of the casting, reduces the concentration of additives introduced to the bronze matrix and hardness. Undertaken research to develop technology of thick-walled products (g> 6 mm) of complex aluminium bronzes. Particular attention was paid to the metallurgy of granules. As a result, a large cooling speed of the alloy, and also high-speed solidification casting a light weight of the granules allows: to avoid micro-and macrosegregation, decreasing the particle size, increase the dispersion of phases in multiphase alloys. Depending on the size granules as possible is to provide finished products with a wall thickness greater than 6 mm by infiltration of liquid alloy of granules (composites). Preliminary studies was conducted using drip method granulate of CuAl10Fe5Ni5 bronze melted in a INDUTHERM-VC 500 D Vacuum Pressure Casting Machine. This bronze is a starting alloy for the preparation of the complex aluminium bronzes with additions of Cr, Mo, W and C or Si. Optimizations of granulation process was carried out. As the process control parameters taken a casting temperature t (°C) and the path h (mm) of free-fall of the metal droplets in the surrounding atmosphere before it is intensively cooled in a container of water. The granulate was subjected to a sieve analysis. For the objective function was assume maximize of the product of Um*n, the percentage weight "Um" and the quantity of granules 'n' in the mesh fraction. The maximum value of the ratio obtained for mesh fraction a sieve with a mesh aperture of 6.3 mm. In the intensively cooled granule of bronze was identified microstructure composed of phases: β and fine bainite (α+β'+β'1) and a small quantity of small precipitates κII phase. Get high microhardness bronze at the level of 323±27,9 HV0,1.
Go to article

Abstract

This paper describes the possibility of using very short periods of solution annealing in the heat treatment of unmodified hypoeutectic silumin alloy AlSi7Mg0,3 casted by method of casting with crystallization under pressure with forced convection (direct squeeze casting process). Castings prepared at different casting parameters were subjected to special heat treatment called SST (Silicon Spheroidization Treatment), which were originally used only for the modified silumin alloys to spheroidization of eutectic silicon. Temperature holding time in solution annealing of T6 heat treatment is limited in the SST process to only a few minutes. It was studied the effect of casting parameters and periods of solution annealing on ultimate strength, yield strength, and especially ductility that in the unmodified silumin alloy castings is relatively low.
Go to article

Abstract

This study presents an analysis of aluminium cast iron structure (as-cast condition) which are used in high temperatures. While producing casts of aluminium iron, the major influence has been to preserve the structure of the technological process parameters. The addition of V, Ti, Cr to an Fe-C-Al alloy leads to the improvement of functional and mechanical cast qualities. In this study, a method was investigated to eliminate the presence of undesirable Al4C3 phases in an aluminium cast iron structure and thereby improve the production process. V and Ti additions to aluminium cast iron allow the development of FeAl - VC or TiC alloys. In particular, V or Ti contents above 5 wt.% were found to totally eliminate the presence of Al4C3. In addition, preliminary work indicates that the alloy with the FeAl - VC or TiC structure reveals high oxidation resistance. The introduction of 5 wt.% chromium to aluminium cast iron strengthened the Al4C3 precipitate. Thus, the resultant alloy can be considered an intermetallic FeAl matrix strengthened by VC and TiC or modified Al4C3 reinforcements.
Go to article

Abstract

The aim of this publication is to present practical application of the R. Kolman’s quality rating method used in the evaluation of aluminium alloys. The results of studies of the mechanical and physical properties of the three selected test materials are discussed. To find the best material, the quality level of each of the tested materials was assessed using quality ratings proposed by R. Kolman. The results of the conducted analysis have proved that the best material was an AKII MM alloy, i.e. a casting AK11 aluminium alloy from the 4XXX series.
Go to article

Abstract

The work deals with technology Patternless process that combines 3 manufacturing process mold by using rapid prototyping technology, conventional sand formation and 3D milling. It's unconventional technology that has been developed to produce large-sized and heavyduty castings weighing up to several tons. It is used mainly in prototype and small batch production, because eliminating production of models. The work deals with the production of blocks for making molds of gypsum and gypsum drying process technology Thermomold. Into blocks, where were made cavities by milling were casted test castings from AlSi10MgMn alloy by gravity casting. At machining of the mold cavity was varied feed rate of tool of cemented carbide. Evaluated was the surface roughness of test castings, that was to 5 micrometers with feed from 900 to 1300 mm/min. The dimensional accuracy of castings was high at feed rate of 1000 and 1500 mm/min did not exceed 0.025 mm.
Go to article

Abstract

The study presents the results of the investigations of the effect of Cu, Ni, Cr, V, Mo and W alloy additions on the microstructure and mechanical properties of the AlSi7Mg0.3 alloy. The examinations were performed within a project the aim of which is to elaborate an experimental and industrial technology of producing elements of machines and devices complex in their construction, made of aluminium alloys by the method of precision investment casting. It was demonstrated that a proper combination of alloy additions causes the crystallization of complex intermetallic phases in the silumin, shortens the SDAS and improves the strength properties: Rm, Rp0.2,HB hardness. Elevating these properties reduces At, which, in consequence, lowers the quality index Q of the alloy of the obtained casts. Experimental casts were made in ceramic moulds preliminarily heated to 160 °C, into which the AlSi7Mg0.3 alloy with the additions was cast, followed by its cooling at ambient temperature. With the purpose of increasing the value of the quality index Q, it is recommended that the process of alloy cooling in the ceramic mould be intensified and/or a thermal treatment of the casts be performed (ageing)(T6).
Go to article

Abstract

The paper presents data concerning the total production of castings over the 2000-2014 period, both on a global scale, and in Poland. The basic types of casting alloys were taken into account. Changes in the production volume and structure over the period of the analysed 15 years were pointed out with respect to countries leading in foundry production. The topmost position in the world foundry industry is held by China for several years (with almost 45% share in the foundry market), the second place is taken by India (with almost 9% share). A distinct reduction in the shares of the once significant producers of castings, such as USA, Japan, Germany, Russia, Italy, or France, was observed over the 2000-2014 period. Poland had a share of 1.16% in 2000, and of 1.02% in 2014. Comparing the detailed data concerning the years 2000 and 2014, one can see that the fractions of castings made of ductile iron, cast steel, aluminium alloys, or magnesium alloys increase on a global scale, while such alloys as grey cast iron or malleable are in decline.
Go to article

Abstract

Metal alloys with matrix based on an Fe-Al system are generally considered materials for high-temperature applications. Their main advantages are compact crystallographic structure, long-range ordering and structural stability at high temperatures. These materials are based on an intermetallic phase of FeAl or Fe3Al, which is stable in the range from room temperature up to the melting point of 1240°C. Their application at high temperatures is also beneficial because of the low cost of production, very good resistance to oxidation and corrosion, and high mechanical strength. The casting alloy the structure of which includes the FeAl phase is, among others, highaluminium cast iron. This study has been devoted to the determination of the effect of vanadium and titanium on the transformation of the high-aluminium cast iron structure into an in-situ FeAl-VC composite.
Go to article

Abstract

The article presents the investigation results of the crystallization (performed by means of the TDA method) and the microstructure of complex aluminium bronzes with the content of 6% Al, 4% Fe and 4% Ni, as well as Si additions in the scope of 1–2% and Cr additions in the scope of 0.1–0.3%, which have not been simultaneously applied before. For the examined bronze, the following tests were performed: hardness HB, impact strength (KU2). For bronze CuAl6Fe4Ni4Si2Cr0.3, characterizing in the highest hardness, wear tests were conducted with dry friction and the dry friction coefficient. The investigations carried out by means of the X-ray phase analysis demonstrated the following phases in the microstructure of this bronze: αCu, γ2 and complex intermetallic phases based on iron silicide type Fe3Si (M3Si M={Fe,Cr,…}). Compared to the normalized aluminium bronzes (μ=0.18–0.23), the examined bronze characterizes in relatively low wear and lower friction coefficient during dry friction (μ=0.147±0.016).
Go to article

Abstract

US A356 and US 413 cast aluminium alloys shrinkage characteristic have been discussed in the present study. Specific volume reduction leads to shrinkage in castings and it can be envisaged as a casting defect. Finite difference based casting process simulation software has been used to study the shrinkage characteristic and it is quantified using mathematical formulae. The three dimensional model of the shrinkage defect has been constructed using CAD application software. Shrinkage characteristic has also been quantified through experimental validation studies and compared well with casting process simulation. Shrinkage characteristic study and control is essential for producing defect free castings. Influence of casting shape on the shrinkage characteristic has been studied in this paper.
Go to article

Abstract

The work presents the investigation results concerning the structure of composite pressure die castings with AlSi11 alloy matrix reinforced with SiC particles. Examination has been held for composites containing 10 and 20 volume percent of SiC particles. The arrangement of the reinforcing particles within the matrix has been qualitatively assessed in specimens cut out of the castings. The index of distribution was determined on the basis of particle count in elementary measuring fields. The tensile strength, the yield point and elongation of the obtained composite were measured. Composite castings were produced at various values of the piston velocity in the second stage of injection, diverse intensification pressure values, and various injection gate width values. The regression equation describing the change of the considered arrangement particles index and mechanical properties were found as a function of the pressure die casting parameters. The infuence of particle arrangement in composite matrix on mechanical properties these material was examined and the functions of correlations between values were obtained. The conclusion gives the analysis and the interpretation of the obtained results.
Go to article

Abstract

The paper presents the results of investigations concerning the influence of negative (relative) pressure in the die cavity of high pressure die casting machine on the porosity of castings made of AlSi9Cu3 alloy. Examinations were carried out for the VertaCast cold chamber vertical pressure die casting machine equipped with a vacuum system. Experiments were performed for three values of the applied gauge pressure: -0.3 bar, -0.5 bar, and -0.7 bar, at constant values of other technological parameters, selected during the formerly carried initial experiments. Porosity of castings was assessed on the basis of microstructure observation and the density measurements performed by the method of hydrostatic weighing. The performed investigation allowed to find out that – for the examined pressure range – the porosity of castings decreases linearly with an increase in the absolute value of negative pressure applied to the die cavity. The negative pressure value of -0.7 bar allows to produce castings exhibiting porosity value less than 1%. Large blowholes arisen probably by occlusion of gaseous phase during the injection of metal into the die cavity, were found in castings produced at the negative pressure value of -0.3 bar. These blowholes are placed mostly in regions of local thermal centres and often accompanied by the discontinuities in the form of interdendritic shrinkage micro-porosity. It was concluded that the high quality AlSi9Cu3 alloy castings able to work in elevated temperatures can be achieved for the absolute value of the negative pressure applied to the die cavity greater than 0.5 bar at the applied set of other parameters of pressure die casting machine work.
Go to article

Abstract

To investigate the impact of various Al-Ti-B grain-refiners on solidification and grain-refining performance, a wrought aluminium alloy AA6182 was used. Three different grain-refiners from different manufacturers were used to establish the efficiency, i.e. contact time before casting, on the primary solidification and grain formation size. The primary solidification of α-Al grains at inoculation was observed by using thermal analysis (TA). Differential scanning calorimetry (DSC) was used in order to analyze the quality of various grain-refiners. The size of the primary grains was analyzed using optical microscopy (OM). Scanning electron microscopy (SEM) was used to estimate the size and distribution of Al3Ti and TiB2 particles in various grain-refiners and to establish the best efficiency of the investigated grain-refiners. Within 1-4 min of inoculation the smallest fine equiaxed grains were achieved when either one of the investigated grain-refiners was added. It was established, that grain-refiner A contains higher content of impurities which do not melt in the experimental temperature range made by DSC method. The most pure grain-refiner turned out to be grain-refiner B, in which the most optimal number of TiB2 particles and particle size distribution was found.
Go to article

Abstract

For the die casting conditions of aluminium bronzes assumed based on the literature data, a thick-walled bush was cast, made of complex aluminium bronze (Cu-Al-Fe-Ni-Cr). After the cast was removed from the mould, cracks were observed inside it. In order to identify the stage in the technological production process at which, potentially, the formation of stresses damaging the continuity of the microstructure created in the cast was possible (hot cracking and/or cold cracking), a computer simulation was performed. The article presents the results of the computer simulation of the process of casting the material into the gravity die as well as solidifying and cooling of the cast in the shape of a thick-walled bush. The simulation was performed with the use of the MAGMA5 program and by application of the CuAl10Ni5,5Fe4,5 alloy from the MAGMA5 program database. The results were compared with the location of the defects identified in the actual cast. As a result of the simulation of the die-casting process of this bush, potential regions were identified where significant principal stresses accumulate, which can cause local hot and cold cracking. Until now, no research has been made of die-cast aluminium bronzes with a Cr addition. Correlating the results of the computer simulation validated by the analysis of the actual cast made it possible to clearly determine the critical regions in the cast exposed to cracking and point to the causes of its occurrence. Proposals of changes in the bush die casting process were elaborated, in order to avoid hot tearing and cold cracking. The article discusses the results of preliminary tests being a prologue to the optimization of the die-casting process parameters of complex aluminium bronze thick-walled bushs.
Go to article

Abstract

Small additions of Cr, Mo and W to aluminium-iron-nickel bronze are mostly located in phases κi (i=II; III; IV),and next in phase α (in the matrix) and phase γ2. They raise the temperature of the phase transformations in aluminium bronzes as well as the casts’ abrasive and adhesive wear resistance. The paper presents a selection of feeding elements and thermal treatment times which guarantees structure stability, for a cast of a massive bush working at an elevated temperature (650–750°C) made by means of the lost foam technology out of composite aluminium bronze. So far, there have been no analyses of the phenomena characteristic to the examined bronze which accompany the process of its solidification during gasification of the EPS pattern. There are also no guidelines for designing risers and steel internal chill for casts made of this bronze. The work identifies the type and location of the existing defects in the mould’s cast. It also proposes a solution to the manner of its feeding and cooling which compensates the significant volume contraction of bronze and effectively removes the formed gases from the area of mould solidification. Another important aspect of the performed research was establishing the duration time of bronze annealing at the temperature of 750°C which guarantees stabilization of the changes in the bronze microstructure – stabilization of the changes in the bronze HB hardness.
Go to article

Abstract

The presented work is aimed to deal with the influence of changes in the value of negative (relative) pressure maintained in the die cavity of pressure die casting machine on the surface quality of pressure castings. The examinations were held by means of the modified Vertacast pressure die casting machine equipped with a vacuum system. Castings were produced for the parameters selected on the basis of previous experiments, i.e. for the plunger velocity in the second stage of injection at the level of 4 m/s, the pouring temperature of the alloy equal to 640°C, and the die temperature of 150°C. The examinations were carried on for three selected values of negative gauge pressure: - 0.03, - 0.05, and - 0.07 MPa. The quality of casting was evaluated by comparing the results of the surface roughness measurements performed for randomly selected castings. The surface roughness was measured by means of Hommel Tester T1000. After a series of measurements it was found that the smoothest surface is exhibited by castings produced at negative gauge pressure value of - 0.07 MPa.
Go to article